GS-10
Click here for Printable data sheet |
GS-30
Click here for Printable data sheet |
GS-40
Click here for Printable data sheet |
GS-50
Click here for Printable data sheet |
GS-70
Click here for Printable data sheet |
||||
| Maximal partikelstorlek | tum | 0.008 | 0.008 | 0.031 | 0.008 | 0.031 | ||
| mm | 0.2 | 0.2 | 0.8 | 0.2 | 0.8 | |||
| Skenbar densitet | pund/fot³ | 98.6 | 109.2 | 107.4 | 106.1 | 108.0 | ||
| g/cc³ | 1.58 | 1.75 | 1.72 | 1.70 | 1.73 | |||
| Specifik elektrisk resistans | x 10-5 ohm | 82.0 | 38.0 | 25.0 | 25.0 | 26.0 | ||
| x 10-6 ohm | 20.8 | 9.7 | 6.4 | 6.4 | 6.6 | |||
|
Böjnings styrka (WG) (Fyrpunkts-belastning) |
pund/tum² | 2400 | 3300 | 2700 | 2700 | 2205 | ||
| N / mm² | 16.5 | 22.7 | 18.6 | 18.6 | 15.2 | |||
| Kompressions styrka (WG) | pund/tum² | 6100 | 6850 | 6000 | 5700 | 4750 | ||
| N / mm² | 42.0 | 47.2 | 41.3 | 39.3 | 32.7 | |||
| Värme expansions koefficient | x 10-5 per °F (77 till 212 °F) | 1.05 | 0.47 | 0.55 | 0.60 | 0.33 | ||
| x 10-7 per °C (25 till 100 °C) | 1.91 | 0.85 | 1.00 | 1.09 | 0.60 | |||
| Värme lednings förmåga (WG) | BTU / fot-h-°F | 20.3 | 74.8 | 86.8 | 82.5 | 98.3 | ||
| W / m-°C | 35.1 | 129.4 | 150.2 | 142.8 | 170.0 | |||
| Aska | % | 0.25 | 0.10 | 0.10 | 0.10 | 0.10 | ||
| Ovanstående värden är typiska och ska inte användas som specifikationsgränser om inte annat anges. Uppgifterna om de typiska egenskaperna uppdateras rutinmässigt. För att få de senaste uppgifterna besök vår hemsida på www.ozarkgraphite.com. | ||||||||